ACI R Cement and Concrete Terminology Reported by ACI Committee Hamid Farzam Chairman Glen Bollin Bernard J. Erlin Fred. Note: A newer version of this document exists. This document was replaced by R ICRI and ACI member, he serves on several committees including. , Construction American Concrete Institute Committee , “ACI R, Cement and.
Author: | Nagor Mikacage |
Country: | Belarus |
Language: | English (Spanish) |
Genre: | Technology |
Published (Last): | 22 March 2013 |
Pages: | 418 |
PDF File Size: | 8.88 Mb |
ePub File Size: | 12.64 Mb |
ISBN: | 677-3-46237-996-9 |
Downloads: | 74724 |
Price: | Free* [*Free Regsitration Required] |
Uploader: | Negal |
See also abrasion damage and cavitation damage. See also sway brace and X-brace. See also creep; and creep, drying. See also deformation, inelastic.
ACI R Cement and Concrete Terminology 水泥和混凝土术语_百度文库
See also moist room. See also factor, Philleo. See also beam, spandrel; girder; girt; joist; ledger; purlin; and stringer. See also biological shielding. See also hod and mortar board. See also centrifugal process. This occurs because no term has been discarded if there was reason to believe it would appear to be technical in nature to a casual reader of the ACI literature.
See also concrete, architectural. See also expansion, shortening, and swelling. See also flow, capillary. For drafting this edition, all members, both associates and voting, participated. See creep; and creep, basic.
See also concrete, lean. See also contraction; expansion; creep; length change; volume change; shrinkage; deformation, inelastic; and deformation, time-dependent. See also checking and cracks.
See also foundation, mat. See also jointer [concrete]. I ignition loss—see loss on ignition preferred term. See also curing and curing, membrane. See also moisture, surface. See also cement paste, neat.
See also bat; bolster, slab; chair. See also standard deviation. See also water-cement ratio. See also alite; belite; felite; and brownmillerite. See adi coupling sleeve, end-bearing sleeve, mechanical connection. See also ack, well-graded. See also acu, preshrunk.
See also disintegration and weathering. See also mesh, diamond. See also bar support. See also belite, celite, and felite. See also column, slender. See also crusher, primary. Kelly ball test—see test, ball and Kelly ball. See also deterioration and weathering. See also aggregate, gap-graded. See also mud slab and subbase.
Gunite—a proprietary term for shotcrete. E early ages of concrete —the period following the time of final setting during which properties are changing rapidly and heat evolution is important; for concrete made with Type I cement stored moist at 73 F 23 Cit is the first 72 h.
International Concrete Abstracts Portal
Each definition shall be stated in one sentence; 2. See also concrete, zero-slump and concrete, negative-slump. See also foundation, raft. See also bond 1116r and oil, form. L lacing—horizontal bracing between shoring members.
See also dicalcium silicate and tricalcium silicate. See also clinker, portand-cement. It recognizes, however, that the listing may not be complete and that some definitions may be at variance with some commonly accepted aic.
Atterberg limits—see limits, Atterberg. See also damage, abrasion, and erosion.